Separated from the slag,the molten iron is tapped(分流)from the bottom of the furnace. Running from troughs(槽),into specially lined,pure ladle cars(钢水 罐车) The basic oxygen furnaces (BOF's)can produce a heat (>200 tons of prime steel)in 35-50 min.Here begins the intricate process of refining the iron into custom tailored steel
Separated from the slag, the molten iron is tapped(分流) from the bottom of the furnace. Running from troughs(槽), into specially lined, pure ladle cars(钢水 罐车). The basic oxygen furnaces (BOF's) can produce a heat (>200 tons of prime steel) in 35-50 min. Here begins the intricate process of refining the iron into custom tailored steel
Casting Molten steel flows into the casters water cooled mold,where it begins to solidify and take shape. Continuous casting enhances quality, conserves energy,and boosts productivity and yield
Casting Continuous casting enhances quality, conserves energy, and boosts productivity and yield. Molten steel flows into the casters water cooled mold, where it begins to solidify and take shape